classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-123 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-01 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 |
filingDate | 2004-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007500276-A |
titleOfInvention | Molded filling composition with reduced spray mark and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To reduce or eliminate surface defects of a spray mark observed during molding of a mineral-filled polymer material while maintaining good physical properties of an article manufactured from the filled polymer material. SOLUTION: Poly (arylene ether), polyamide, polycarbonate, polyetherimide, polysulfone, polyketone, poly (alkenyl aromatic), poly (alkenyl aromatic) copolymer, polyolefin or a blend of two or more of these polymeric materials or A composition comprising a polymeric material comprising a compatibilized blend, a mineral filler, and about 1 part by weight or more of carbon black based on the total weight of the composition. It has been found that molded articles made from compositions containing carbon black exhibit reduced spray marks when compared to corresponding compositions that do not contain carbon black. Also provided is a method of reducing the spray marks on a molded article. [Selection] Figure 1 |