http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007333846-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C61-06 |
filingDate | 2006-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_538ceb63d785ddb6db48ed2b7402b76c |
publicationDate | 2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007333846-A |
titleOfInvention | Heat shrink film |
abstract | Heat shrinkable film for use in the production of a retardation film, which can obtain a retardation film having a good balance between orientation in the machine direction (MD) and orientation in the transverse direction (TD) I will provide a. A biaxially oriented polypropylene comprising a propylene-1-butene copolymer having a 1-butene content of 0.1 wt% to 10 wt% and a 20 ° C xylene soluble part content of 3% or less. A film, The horizontal direction (TD) heat shrinkage at 140 ° C. is more than twice the vertical direction (MD) heat shrinkage, and A biaxially stretched polypropylene film having a heat shrinkage in the transverse direction (TD) at 150 ° C. that is at least twice the heat shrinkage in the machine direction (MD). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101612789-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8277950-B2 |
priorityDate | 2006-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.