Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_657f8fe5931a3364fda9ccca712ad398 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-614 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-237 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5264 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5248 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5244 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-656 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6586 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2918 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-294 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-249928 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6562 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62878 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62281 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62272 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62876 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62884 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62873 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-87 |
filingDate |
2007-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69dbe8d786bcca5c4a6ddb8cc49782ce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_683d96accba56f45c8ac6aedd7622448 |
publicationDate |
2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007332020-A |
titleOfInvention |
Article manufacturing method, composition and article |
abstract |
PROBLEM TO BE SOLVED: To provide a relatively low-cost manufacturing method suitable for producing a porous SiC-containing article and an article having a controlled porosity. The method of manufacturing an article of the present invention includes a step of applying a refractory metal in an amount sufficient to form a coating on a carbon-based felt, a temperature sufficient to form a ceramic-based felt, and Thermally processing the refractory metallized carbon-based felt under time conditions and cooling 14 the ceramic-based felt under conditioned atmospheric conditions. [Selection] Figure 7 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102417986-A |
priorityDate |
2006-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |