http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007328248-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47cc435e1d443f13180f7766df104d9d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1339 |
filingDate | 2006-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45767b7800f883b5b8628a7b1b203207 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_20f6fd73333c52530dd0b90822965895 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3348c437460731b3aac51dac67db6de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd3e4d4c821071b77759bc69cb1e3009 |
publicationDate | 2007-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007328248-A |
titleOfInvention | Photosensitive resin composition for liquid crystal spacer, photosensitive element using the same, and method for producing liquid crystal spacer |
abstract | PROBLEM TO BE SOLVED: To increase the sensitivity of a photosensitive element to light having a wavelength of 400 or more and to form a resist pattern with light having a wavelength of 390 nm to 420 nm with sufficient sensitivity and resolution, and a photosensitive resin composition for a liquid crystal spacer. And a method for producing a photosensitive element and a liquid crystal spacer using the same. A liquid crystal display device in which liquid crystal is sealed between substrates disposed to face each other, used as a spacer disposed in order to keep the thickness of a liquid crystal layer in the liquid crystal display device constant, and a wavelength (A) a binder polymer, (b) a photopolymerizable unsaturated compound having at least one ethylenically unsaturated group, and (c) a free radical by active light, capable of forming an image at 405 nm exposure at 200 mJ / cm 2 or less. And (d) a photosensitive resin composition for a liquid crystal spacer having a sensitizing dye, a photosensitive element using the same, and a method for producing a liquid crystal spacer. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013080259-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013092693-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008116751-A |
priorityDate | 2006-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 407.