Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 |
filingDate |
2006-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6cdb91d132bffad3dca626b9f7c09b6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5dcc4856649a518ef2504129187026e |
publicationDate |
2007-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007326948-A |
titleOfInvention |
Film and manufacturing method thereof |
abstract |
PROBLEM TO BE SOLVED: To provide a film excellent in mechanical strength and dimensional stability and a method for producing the film. Particles containing 30 to 52% by weight of an aluminum element having an average minor axis (ASP) of 50 nm or less and a particle size ratio (ALP / ASP) to the average major axis (ALP) of 20 to 1,000. A film characterized by having a coating layer having a thickness of 0.1 to 20 μm made of an acrylic resin containing 1 to 90 parts by weight of at least one surface of a polyester film. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017185777-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017170659-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11623976-B2 |
priorityDate |
2006-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |