http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007308521-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_097405822d505467fd50f7100022cd56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate | 2006-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ed0efbe1beb8316a22a02511e94a813 |
publicationDate | 2007-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007308521-A |
titleOfInvention | Thermoplastic resin composition |
abstract | The present invention provides a thermoplastic resin composition having a high elongation at break and improved mechanical strength such as impact resistance and rigidity under short-term melt-kneading production conditions such as an extruder. SOLUTION: A styrene polymer having 2 or more epoxy groups per molecule 0.1 to 10% by weight, a liquid crystalline thermoplastic resin 1 to 98% by weight, a condensed thermoplastic resin 1 to 98% by weight and a catalyst 0 Use 5 to 500 ppm. A styrene polymer having two or more epoxy groups per molecule is preferably a polymer having a styrene monomer and an epoxy group-containing vinyl monomer as essential components. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023132319-A1 |
priorityDate | 2006-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 113.