http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007308520-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_097405822d505467fd50f7100022cd56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L57-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-12 |
filingDate | 2006-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ed0efbe1beb8316a22a02511e94a813 |
publicationDate | 2007-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007308520-A |
titleOfInvention | Thermoplastic resin composition |
abstract | Thermoplastic resin composition having high elongation at break and improved balance of mechanical strength such as breaking strength, breaking elongation, impact resistance and rigidity under short-term melt-kneading production conditions such as an extruder Offer things. A heat containing a styrene polymer (A) having two or more epoxy groups per molecule, a liquid crystalline thermoplastic resin (B), a vinyl thermoplastic resin (C) and a catalyst (D) as constituent components. A thermoplastic resin composition comprising (A) 0.1 to 10 wt%, (B) 1 to 98 wt%, (C) 1 to 98 wt%, and (D) 0.5 to 500 ppm. Resin composition. [Selection figure] None |
priorityDate | 2006-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 70.