http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007294080-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-708 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-706 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-73 |
filingDate | 2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de21c2892cc969f3c81a59d20a49c640 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73a0dd9fa88c406a91cea09d1fb30290 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59ed69be4ef3117e2191b2225aa47b9e |
publicationDate | 2007-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007294080-A |
titleOfInvention | Magnetic recording medium |
abstract | [PROBLEMS] To provide high-capacity magnetic recording that has excellent durability that does not cause edge damage even when the tape conveyance speed is increased, has no head contamination, has low noise, and is suitable for handling in production processes. Provide media. A magnetic layer containing a ferromagnetic powder and a binder is provided on one side of a nonmagnetic support, and the magnetic layer contains diamond particles having an average particle diameter of 20 to 100 nm. The volume of the support is 100 to 8000 nm 3 and the intrinsic viscosity of the support is 0.40 to 0.60 dl. / G is substantially free of particles. [Selection figure] None |
priorityDate | 2006-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 201.