http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007291366-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-14 |
filingDate | 2007-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_210c8f5e46bf087ec856bc6f49ebb3c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_148d8a60d2f62421d34b8e3d7087bfa2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_063eb686c7e991fdd15bedc73d9f401f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_969496b663f9d1403a15571c0d17a4cb |
publicationDate | 2007-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007291366-A |
titleOfInvention | Resin composition for biaxially oriented styrene resin sheet, and sheet and molded product using the same |
abstract | [PROBLEMS] To improve deep drawing formability and prevention of cracking at the time of trimming without causing poor sheet appearance when forming a biaxially oriented styrene resin sheet, and further, low temperature formability and prevention during secondary forming. Provided are a biaxially stretched styrene-based resin sheet excellent in clouding agent applicability, a molded product using the same, and a resin composition constituting them. SOLUTION: The number of branches per molecule in an absolute molecular weight of 734,000 determined by GPC-MALLS method is 0.04 to 0.35, and the weight average molecular weight (Mw) determined by GPC-MALLS method is 250,000 to 450,000, The ratio of the weight average molecular weight (Mw) to the number average molecular weight (Mn) (Mw / Mn) is 2.20 to 3.00, and the ratio of the weight average molecular weight (Mw) to the peak molecular weight (Mp) determined by the GPC method (Mw / Mp) is 1.05-1.28, and contains a copolymer resin obtained by polymerizing a styrene monomer and an acrylate ester, and a resin composition for a biaxially stretched styrene resin sheet. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011225866-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008248156-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013067752-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013100431-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013100430-A |
priorityDate | 2006-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 152.