Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_faf522b8b83eded745c73018576219ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4e04dd2ffee41f8c3255bd5df99f6d5c |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-355 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-397 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-832 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate |
2006-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_052fc9a8e706d11e5c4e919e2069d55f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3189a34a34a4e128a35d43225f69bb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_479fdf1dc03f1d5d3dde27b5510a809a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2a73cd0e3c76fed3494ce5918a3b3f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec2599d52c78fd24ccc5a3ad0a8f6cc2 |
publicationDate |
2007-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007291213-A |
titleOfInvention |
Recycling method for plastic waste |
abstract |
A plastic waste material in which various types of plastic materials are mixed is reused so that a plastic molded product having mechanical strength can be formed, and recycling of the plastic waste material is promoted. [MEANS FOR SOLVING PROBLEMS] A modifier comprising a mixture of a styrene-based thermoplastic elastomer and fine powder made of calcium carbonate having an average particle size of 0.1 to 0.5 μm is added to a plastic waste material in which various types of plastic materials are mixed. To form a molded product of a predetermined shape. The modifier is formed by mixing 2 to 3 parts by weight of fine powder with respect to 1 part by weight of thermoplastic elastomer. Further, the modifier is added at a ratio of 1 to 20 parts by weight with respect to 100 parts by weight of the plastic waste material. [Selection] Figure 3 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110684283-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3307505-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112210149-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008184534-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10336891-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9969868-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10975228-B2 |
priorityDate |
2006-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |