http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007290268-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61J1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D81-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2006-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49ebd57529af8179a55d18c874eb1c90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49695512147b856b51707b4c16fdec3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c3f80bc324f463dd7079665cfd140c4 |
publicationDate | 2007-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007290268-A |
titleOfInvention | Packaging materials and packaging containers for nutrients using the same |
abstract | PROBLEM TO BE SOLVED: To have both excellent storage stability and contents visibility, and for example, when used as a packaging container for nutrients, the contents can be stored for a long period of time, and the dosage and administration speed of the contents are reduced. Provided is a packaging material that can be precisely adjusted. In a packaging material comprising a base material layer (3) made of a resin film, a heat-sealable resin layer (4), a printing layer (6, 7), and optionally an intermediate layer made of a resin film. , A gas barrier layer (5) is provided on the base material layer or the intermediate layer, and part or all of the packaging material is 20% or less in a wavelength region of 250 nm to 550 nm, and a wavelength region of 650 nm to 800 nm. The packaging material is characterized in that it is a content viewing portion having a light transmittance of 50% or more, and the other portion has a total light transmittance of 20% or less. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015186713-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015186713-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106458420-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106458420-B |
priorityDate | 2006-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 83.