http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007289939-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb35bfe7ceb6ccdc2a0c9b447c0ffda8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 |
filingDate | 2007-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5efd0cf41455bac506bb6d29b9394591 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_628cbbf1c7ab0fd5bb39d535d9191f48 |
publicationDate | 2007-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007289939-A |
titleOfInvention | Manufacturing method of laminate |
abstract | The present invention provides a deep, calm brightness feeling and excellent aesthetics by laminating a specific optical coherent chip having optical coherence on a substrate having irregularities. A laminated body is provided. The manufacturing method of the present invention is an optical interference in which spherical particles having an average particle size of 5 nm to 800 nm and a standard deviation of particle size distribution of 20% or less are regularly arranged on a substrate having irregularities. A color clear paint containing a functional chip and a synthetic resin is applied. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010194449-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008012837-A |
priorityDate | 2006-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |