http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007277771-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_623d02c6091d38f6b59470d9ab8ce72c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-272 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-352 |
filingDate | 2006-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8163cd6e3d7b6e416c8799ffc3ef3cd9 |
publicationDate | 2007-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007277771-A |
titleOfInvention | Antistatic composite material and manufacturing method thereof |
abstract | Disclosed is an antistatic composite material that has excellent antistatic properties and is less affected by coloring due to a conductive material, and a method for producing the same. Disclosed is a composite material in which only one surface of a base material is coated with a conductive material, and the surface resistance value of the coated surface is 1.0 × 10 9 Ω or less. A process of setting the adhesion amount of the monomer to 0.8 to 4.0% o.w.f by applying a solution of the conductive composite material and the conductive polymer-forming monomer to the fiber substrate, or And applying a solution of the conductive polymer-forming monomer to the plastic film or sheet substrate to make the amount of the monomer attached 0.2 to 1.5 g / m 2 , and an oxidizing agent solution. The step of applying to the material, the step of applying the solution of the monomer and the oxidizing agent solution is a step of spraying, coating or printing the solution, and the conductive material obtained by polymerizing the monomer only on one side of the substrate A system characterized by covering with Method for manufacturing a sexual composite material. [Selection figure] None |
priorityDate | 2006-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |