http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007270335-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-02 |
filingDate | 2006-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_992841a05675e180a09a662c9387b05e |
publicationDate | 2007-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007270335-A |
titleOfInvention | Corundum laminate manufacturing method and corundum laminate |
abstract | An object of the present invention is to provide a method for easily producing a corundum laminate in which a corundum layer made of corundum crystals is formed on a substrate. According to the present invention, an aluminum oxide film forming solution in which an aluminum-containing compound having a metal oxide film forming property is dissolved is atomized by a spray device, and the atomized aluminum oxide film forming solution is used. An aluminum oxide film forming step of forming an aluminum oxide film on the substrate by contacting the substrate heated to a temperature equal to or higher than an aluminum oxide film forming temperature, and the aluminum oxide film forming step; And a crystallization step of heating the aluminum oxide film formed on the aluminum oxide film to a corundum crystallization temperature or higher to make the aluminum oxide film a corundum layer made of a corundum crystal. The problem is solved by providing a method. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012053436-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009221051-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009132031-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010209363-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012521312-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012171083-A |
priorityDate | 2006-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 175.