http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007238748-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ebdfc88803aa0e0bb776ddb9db35fda |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 |
filingDate | 2006-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_749146518c5641300c51de3a5b887dcc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36689d48115036127d18e0aa7e898455 |
publicationDate | 2007-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007238748-A |
titleOfInvention | Polypropylene resin composition and molded product thereof |
abstract | An object of the present invention is to reduce the degree of compression in order to eliminate white spots due to poor dispersion of inorganic fillers, so that the amount of air to be brought in increases. Providing talc-containing polypropylene resin composition and its molded products. SOLUTION: A bulk specific gravity of 0.3 to 1.0, a compressibility of 3.1 to 1.0, obtained by degassing and compressing polypropylene resin (A) to 55 to 95% by weight and an average particle size of 0.1 to 12 μm. 7.0 to 45% by weight of degassed compressed talc (B) of 7.0, 100 parts by weight of the total amount of (A) and (B), fatty acid having a melting point of 140 ° C. or lower, or a metal salt thereof (C ) And 0.1 to 1.0 parts by weight of a fatty acid metal salt (D) having a melting point of 150 ° C. or higher, and molding thereof Goods. [Selection figure] None |