Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24975 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0294 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0278 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-118 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 |
filingDate |
2006-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb3e920acb8628477fbe32ebfeb9d20d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5fac8f3b1833bb27d556b2854aa58ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3925e4f7e8e2d626e335707dd89f193 |
publicationDate |
2007-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007233185-A |
titleOfInvention |
Optical film, antireflection film, polarizing plate, and image display device |
abstract |
[PROBLEMS] To obtain an optical film with reduced surface roughness and wind uniformity and high surface uniformity, an antireflection film having both sufficient antireflection performance and scratch resistance, and the above antireflection film with high productivity. To provide a high-speed coating production method and a polarizing plate and an image display device using such an antireflection film. In an optical film having an optical layer on a transparent support, the optical layer contains a thickener, and the viscosity when 3% by mass of the thickener is added to 2-butanone is 10 mPa · sec or more. And an optical film having a thickness of 5 μm or more. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011215552-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010134424-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010085760-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8932669-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013105160-A |
priorityDate |
2006-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |