http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007220652-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-075 |
filingDate | 2006-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_27014e252d3d3b9b91be887e65d63597 |
publicationDate | 2007-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007220652-A |
titleOfInvention | Photosensitive paste |
abstract | The present invention provides a photosensitive paste capable of reducing sensitivity reduction during exposure and capable of forming a dense pattern. A glass particle (B) containing at least one selected from the group consisting of inorganic particles (A) having a softening temperature of 600 ° C. or higher, alkali metal oxides and alkaline earth metal oxides (B). ), An alkali-soluble resin (C), a compound (D) that generates acid upon irradiation or heating of electromagnetic radiation, and an organic solvent (E), wherein the alkali metal oxide content is photosensitive. The photosensitive paste characterized by being 2 mass% or less by mass fraction with respect to the conductive paste, or 3 mass% or less by mass fraction with respect to the glass particles (B). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016015398-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008035785-A1 |
priorityDate | 2005-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 434.