http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007199581-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-163 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09G3-20 |
filingDate | 2006-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_786a725f92cd885137098b37f9689102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc5678e553036d5d296fa5c8019adde6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0cb9ac8f8f59fd4248748b07547800d7 |
publicationDate | 2007-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007199581-A |
titleOfInvention | Driving method of electrochemical display element |
abstract | PROBLEM TO BE SOLVED: To provide a driving method of an electrochemical display element capable of extending the element life by preventing the occurrence of black spots. A driving method for an electrochemical display element, which includes a coloring step of applying a reduction voltage on a viewing-side electrode and a decoloring step of applying an oxidation voltage by reversing the polarity of the viewing-side electrode. The oxidation voltage includes at least two voltages: a first voltage step for dissolving most of the deposited metal of the pixel and a second voltage step for erasing the minute metal nuclei remaining in a part of the pixel. And the first voltage step is a voltage step for applying the voltage V1, and the second voltage step is (1) a voltage step for applying a voltage V2 satisfying V1 <V2 following the voltage V1, or (2) A method for driving an electrochemical display element, which is a voltage step of applying a voltage V3 where V1 ≦ V3 after applying a voltage V1 and then passing through an application of an oxidation threshold voltage or less and / or no application of a voltage. . [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009128818-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015093298-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9690163-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105829960-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105829960-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015093298-A1 |
priorityDate | 2006-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 126.