Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2001-12 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K1-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate |
2006-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ddc98902d4a127f6d5e82d8b75c9614 |
publicationDate |
2007-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007176164-A |
titleOfInvention |
Transparent polymer film and method for producing the same, and optical compensation film, laminated film and liquid crystal display device using the same |
abstract |
Disclosed is a transparent polymer film having a high elastic modulus, a small humidity dimensional change, and an appropriate moisture permeability. A transparent polymer film having a moisture permeability of 100 g / (m 2 · day) or more in terms of a film thickness of 80 μm at 40 ° C. and a relative humidity of 90% is stretched by 10% or more at (Tg + 50) ° C. or more. Manufacturing. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2013187134-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010078909-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009119808-A |
priorityDate |
2005-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |