http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007173254-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0e7f7286c46e676b1bc0daf37b9f6c63 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 |
filingDate | 2007-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd432ee812e22b7a03ac8a6064bd41e2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a10f45fc3c6e8bfac5d0e35965082cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dcbc4967808cd03529b38ac648816a2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_30bdf800d62a9530a5da610e59031d1c |
publicationDate | 2007-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007173254-A |
titleOfInvention | Alkaline battery |
abstract | PROBLEM TO BE SOLVED: To provide an alkaline battery having excellent load characteristics and preventing gas generation and storage stability from being reduced by reaction with an electrolytic solution, while suppressing heat generation behavior when an abnormality occurs. SOLUTION: A positive electrode mixture containing at least one of manganese dioxide and nickel oxide, a conductive agent and an alkaline electrolyte (A) in which potassium hydroxide is dissolved, a separator, and a zinc alloy powder, a gelling agent, and hydroxylation An alkaline battery produced by enclosing a negative electrode mixture containing an alkaline electrolyte (B) in which potassium is dissolved in an exterior body, wherein the potassium hydroxide of the alkaline electrolyte (A) of the positive electrode mixture The concentration is 45% by mass or more, the potassium hydroxide concentration of the alkaline electrolyte (B) of the negative electrode mixture is 35% by mass or less, and the powder passing through a 200 mesh sieve is used as the negative electrode zinc alloy powder. An alkaline battery using a zinc alloy powder having a ratio of 4 to 40% by mass. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009170157-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009151958-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011138642-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004139909-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010218946-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010010012-A |
priorityDate | 2007-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |