Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294881271413951a95f284b588a68e66 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 |
filingDate |
2005-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f020a69be51780465295acb27b3110e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62a9ca2886f1ee4a3034093e2928170a |
publicationDate |
2007-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007172969-A |
titleOfInvention |
battery |
abstract |
A battery capable of improving the characteristics even in a high temperature environment or a low temperature environment is provided. An electrolyte layer includes an electrolytic solution and a polymer compound that holds the electrolytic solution, and has a so-called gel shape. The electrolytic solution contains an aromatic compound such as ethylene carbonate, propylene carbonate, and diphenyl ether. The content of the low dielectric constant solvent in the electrolytic solution is 3% by volume or less. The polymer compound contains a polymer containing vinylidene fluoride as a component, such as a copolymer of vinylidene fluoride and hexafluoropropylene. [Selection] Figure 2 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010257704-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9819052-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106450459-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008262901-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106340674-A |
priorityDate |
2005-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |