http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007161513-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8117e24b32e11aec60940a0388ad28ed |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-70 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28C7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 |
filingDate | 2005-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3051cd63b34df2e194b3a0dd08ccc3e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e00a79a2141cbf6dc0d2ccd958c0431b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2fec4e548a85bf38773495e51d39d37d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dc759dfa20124e547bf7fb1e153f72e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4abffdd736f4a1595171ebd664b6a578 |
publicationDate | 2007-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007161513-A |
titleOfInvention | PC grout and its manufacturing method |
abstract | The present invention provides a PC grout which can be kneaded and injected with the same equipment as a general grout and can greatly reduce the generation of residual air in a duct. When producing a PC grout comprising a binder and water mixed with a chemical admixture and a thickening admixture, the water admixture ratio is 30 to 70%, and the thickening admixture is as follows. An admixture containing a first water-soluble low molecular weight compound (A) selected from cationic surfactants and a second water-soluble low molecular weight compound (B) selected from anionic aromatic compounds is used as a unit water amount. 0.1 to 3.0% by weight of the mixture, and as the chemical admixture, the carboxyl group-containing polyether water reducing agent is 0.1 to 2.0% by weight of the cement. It mix | blended in the ratio. [Selection figure] None |