http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007160904-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_132721b781afede2175d04e894580568 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C51-14 |
filingDate | 2005-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7a68a1f12985142d4f926292481635f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d5bf909317cd642c1c3f35ec7397898 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61e74b3d5cc80aa694a6ca2becce5229 |
publicationDate | 2007-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007160904-A |
titleOfInvention | Co-extrusion laminated foam and molded product thereof |
abstract | An object of the present invention is to provide a foam having a high antistatic property, capable of being repeatedly used, and having a good balance of mechanical properties, buffer properties and thermoformability, and a molded product having a large unfolding ratio by thermoforming. A polystyrene resin composition foam layer having an apparent density of 300 to 550 g / L, a thickness of 2.0 to 3.5 mm, and an open cell ratio of 40% or less, and having a basis weight of 10 to 100 g / m 2 containing an antistatic agent on at least one side. a polyolefin resin layer, total basis weight is a beyond 1500 g / m 2 or less of the laminated foam 650 g / m 2, a polystyrene resin composition constituting the foam layer contains a styrene-based elastomer, and The rubber component content in the resin composition is 9 to 30% by weight, the surface resistivity of the laminated foam polyolefin resin layer surface after washing with an aqueous ethanol solution is 1 × 10 13 Ω or less, the surface of the foam layer The bubbles in the inner layer part exceeding 25% of the total thickness are 0.6 ≦ between the average bubble diameter A (mm) in the thickness direction, the average bubble diameter B (mm) in the extrusion direction, and the average bubble diameter C (mm) in the width direction. A / B ≦ 1.2 and 0.6 ≦ A / C ≦ 1.2 are satisfied. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7112229-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020174792-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7188896-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020138402-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017113929-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015189052-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019171819-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7132153-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112074403-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112074403-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019189452-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009038059-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011104901-A |
priorityDate | 2005-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.