http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007145987-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-12 |
filingDate | 2005-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a29cb4caf3dbb7ca60e66c1a6d467c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d48249832e4af4c0460279c8a432aa0 |
publicationDate | 2007-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007145987-A |
titleOfInvention | Cyclic olefin copolymer resin extruded foam and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a lightweight thermoplastic resin extruded foam which is excellent in heat resistance, is capable of material recycling and is excellent in environmental compatibility, and can be used for applications requiring dimensional stability in a high temperature atmosphere. Provide the body. SOLUTION: A cyclic olefin copolymer resin and a cyclic olefin copolymer resin extruded foam containing a non-fluorocarbon foaming agent having a foam thickness of 10 to 150 mm, a foam density of 20 to 50 kg / m 3 , and a foam. A cyclic olefin copolymer resin extruded foam having a volume change rate of −10 to + 10% when heated at 100 ° C. under an ambient temperature for 24 hours. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010001459-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2465961-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2465962-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008007785-A1 |
priorityDate | 2005-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.