http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007145956-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-199 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2005-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4cae5738100d5a472ae7e2aa47fdb9c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e7477d23ffe31bb95cf719c57408b80 |
publicationDate | 2007-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007145956-A |
titleOfInvention | Polyester resin and polyester film |
abstract | PROBLEM TO BE SOLVED: To provide a heat-shrinkable polyester film which is less likely to cause whitening, shrinkage spots, wrinkles and distortion when mounted on a body to be mounted, has excellent solvent adhesion, and has good ink releasability with an alkaline aqueous solution. Provide suitable polyester resin. SOLUTION: At least one polyester film containing a polyester resin comprising an acid component containing 3 to 9 mol% adipic acid units and an alcohol component containing 10 to 15 mol% 1,4-cyclohexanedimethanol units. A heat-shrinkable polyester film stretched in the direction. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012512278-A |
priorityDate | 2005-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 85.