http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007119579-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_60c4c585c1866483c4b2cd74ddb4b231 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 |
filingDate | 2005-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ffdcb248f3640a3356214f5ae21b491 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d90679fb0553bf42c943ec423c162c42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_660b85897d2743ba977dcdc4c6c62337 |
publicationDate | 2007-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007119579-A |
titleOfInvention | Thermoplastic polyhydroxy polyether resin and use thereof |
abstract | [PROBLEMS] To provide a thermoplastic polyhydroxy polyether resin and an epoxy resin composition having low elasticity and low stress at room temperature, a glass transition point exceeding 90 ° C., and a high elastic modulus retention at high temperature. . A thermoplastic polyhydroxy polyether resin having a molecular weight of 10,000 to 200,000 and containing a fluorene skeleton as a constituent component and having a molecular weight of 10,000 to 200,000 and an organosiloxane as a constituent component is formed. Heat resistant insulation film. [Selection figure] None |
priorityDate | 2005-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |