http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007078885-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 |
filingDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_04d42e1df67b7d5a40efc6698479ab2c |
publicationDate | 2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007078885-A |
titleOfInvention | Optical sheet for display and manufacturing method thereof |
abstract | An optical sheet, an optical sheet for display, and an optical sheet for display that are suitable for manufacturing with a simple process and high quality without lowering the adhesive strength when optical sheets are bonded to each other. Provide a method. SOLUTION: An optical sheet 12, 14, 16, 18 having a sheet planar size equal to or larger than a product size is coated with an aqueous solution containing a water-soluble antistatic agent and a fluorosurfactant, and the thickness after drying is 0.03. After forming a coating film in a range of ˜0.2 g / m 2 and laminating the optical sheets, the optical sheets are bonded to each other at at least one joint 10A, and the optical sheets are laminated after bonding. Cut the periphery of the body into product size. [Selection] Figure 7 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009116530-A1 |
priorityDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 44.