http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007077212-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7de9ee571d51f83d822588ac9c7b250 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_77702c1ce54414fc07700422641a6883 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268d5d3c08af0ef0c4c3db824c61055e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b67efc8b988e11e7558e9c2ac364b8f5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-10 |
filingDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe959f46989dfc21e7b425136bc8b55e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc613527099700842b29d56c71e90a30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d19b2e78428758b1ea105c0a06f8291e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2bf2bdb7bd4627e3d13f528b0dde59c0 |
publicationDate | 2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007077212-A |
titleOfInvention | Resin material, resin material manufacturing method, use of granular materials |
abstract | PROBLEM TO BE SOLVED: To provide a resin material rich in functionality that can contribute to the next generation global environment, industry, etc., a manufacturing method for producing the resin material, and use of granular materials. SOLUTION: The granular material of the present invention serves as a nucleus for promoting crystallization of a resin, can provide a resin material having excellent crystallinity, and is the same kind of resin material that does not disperse a granular material having a particle size of 50 to 800 nm. In comparison, it is possible to ensure twice or more strength. By securing such a strength of more than twice, the same strength can be realized with a resin material with a thickness of 1/2 or less than the conventional one, so the amount of resin can also be reduced to less than half and can be greatly reduced, so Can greatly contribute to the solution of resource problems. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013122020-A |
priorityDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 505.