http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007062200-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14df928cce1112b89356928855b60351 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K1-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2005-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_532f68b52b9c879b402201c134502246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58e5769fbb54d9125e4ab909e46482ae |
publicationDate | 2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007062200-A |
titleOfInvention | Cellulose ester film, production method thereof, and liquid crystal display device using cellulose ester film |
abstract | PROBLEM TO BE SOLVED To provide a cellulose ester film used as a protective film for a liquid crystal display element, that is, a polarizing plate in the sense of widening the viewing angle of a liquid crystal display device (LCD) operating in an IPS mode capable of realizing an easy-to-view display having a high contrast ratio over a wide range The present invention provides a cellulose ester film having a small birefringence suitable for a protective film for a polarizing plate. SOLUTION: A method for producing a cellulose ester film by a solution casting film forming method, wherein a step of mixing a non-chlorine organic solvent, a cellulose ester, and a retardation reducing additive is obtained in the production of a dope. The mixture is subjected to a step of cooling the mixture at −100 to −10 ° C. and a step of treating the mixture after the cooling treatment at 0 to 120 ° C. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010046834-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5617922-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014055300-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011158626-A1 |
priorityDate | 2005-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 227.