Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b5d58119b48e6e6ae449afc394066f3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-80 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D25-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D25-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate |
2005-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2fd6c3d410eda5029456262ce9003ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7316760a32310c759bba6fb42cfddf4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73c529ffdedb821822499cfd485d5358 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6878b3ba5b08d835b4616ae593a2e5af |
publicationDate |
2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007062056-A |
titleOfInvention |
Heat-shrinkable laminated film, molded product using the film, heat-shrinkable label, and container equipped with these |
abstract |
PROBLEM TO BE SOLVED: To provide a heat-shrinkable laminated film, a heat-shrinkable label, which has excellent film stiffness (rigidity at room temperature), shrinkage finish, transparency at the time of regeneration addition, small natural shrinkage, and sufficient delamination delamination A container with the label is provided. SOLUTION: A rubber obtained by dispersing a rubber-like elastic body in a continuous phase of a copolymer comprising (I) a polyester resin as a main component and a styrene monomer and a (meth) acrylic acid ester monomer. (II) layer mainly comprising a styrene-based thermoplastic resin having a styrene-based hydrocarbon content of 5 to 50% by mass between the layer-like elastic-dispersed polystyrene-based resin (III) layer A laminated film composed of at least three layers having a thermal shrinkage rate of 20% or more in at least one direction when immersed in warm water at 80 ° C. for 10 seconds is formed. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010044163-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008129598-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009285892-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009006530-A |
priorityDate |
2005-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |