http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007035346-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_35f1bf7625ec038f633e972977ad7a70 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 |
filingDate | 2005-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7afbc5f9708383e9a631da5049898684 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38d5fb711b50c297089cb4d6b03a1643 |
publicationDate | 2007-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007035346-A |
titleOfInvention | Electrically conductive material comprising terbium, bismuth, tungsten oxide solid solution and method for producing the same |
abstract | A general formula Tb having a structure provided A monoclinic new material consisting of an oxide solid solution 2x Bi 2y W z O 3 ( 0.66 <x <0.73,0.13 5 <y <0.19, 0.11 <z <0.175, where x + y + z = 1), an electrically conductive material comprising a terbium-bismuth-tungsten oxide solid solution. For example, x = 0.6725, y = 0.17, z = 0. 1575 electrical conductivity 10-4 at 0.99 ° C. In the composition of the S cm- 1, at 250 ° C. 10 3 S cm -1 and has semiconductor properties. Since it exhibits good electrical conductivity, it has applications as materials for electrodes, sensors, catalysts, and the like. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005170783-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104445415-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102008008752-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4649588-B2 |
priorityDate | 2005-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 31.