Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4edd4e526605dbd18b513b4b30d19ab2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2011-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2035-0827 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2791-001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2011-005 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C35-0266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C35-0894 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0003 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-18 |
filingDate |
2005-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1490b64485318b7313f42c7ab144a2f |
publicationDate |
2007-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007015334-A |
titleOfInvention |
Manufacturing method of composite optical element and composite optical element module |
abstract |
PROBLEM TO BE SOLVED: To provide a method for producing a composite optical element with high productivity, in which damage to a mold and a lens substrate caused by adhesion between a mold and a resin layer is small, the thickness of the resin layer can be easily controlled. The present invention relates to a method for producing a composite optical element having a resin layer on the surface of a substrate, the step of applying an ultraviolet curable resin liquid to at least one of the substrate and the mold, A step of adjusting the arrangement of the material and the mold, a step of curing the UV curable resin liquid on the outer periphery of the release facilitating region provided for facilitating release, and an ultraviolet curing in the release facilitating region And a release step of separating the resin layer formed by curing from the mold body. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009279879-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011064871-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009142295-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8956690-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009283093-A |
priorityDate |
2005-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |