http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007015312-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K45-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-02 |
filingDate | 2005-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_28aa916275cb2dd49708145d63a2193d |
publicationDate | 2007-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007015312-A |
titleOfInvention | Manufacturing method of resin molding |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a resin molded body capable of continuously and stably obtaining an optical element which is excellent in low birefringence and requires high precision shape uniformity. A resin material such as a norbornene-based polymer is filled in a mold capable of obtaining a molded body having a height of 5 mm to 40 mm, and the filled resin material is filled with a glass transition temperature Tg (° C.) of the resin material. A method for producing a resin molded body, comprising ejecting from a mold having a temperature α (° C.) lower by 3 to 20 ° C. at an ejection speed S (mm / s) satisfying the relationship of the formula (1). (Α−Tg) × 0.18 + 5.5 ≦ S ≦ (Tg−α) × 0.6 + 18.3 Formula (1) [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016112867-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020011511-A |
priorityDate | 2005-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.