Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e64079869bbb0e5ffa9fc45afaab5395 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16J9-26 |
filingDate |
2005-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d6bbef491db8f15830346d92ead06b02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05789ef94c74663e81f73d45f11a5607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8960f5792ec2f6086c302ec7435cb4ad |
publicationDate |
2007-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007009296-A |
titleOfInvention |
Sliding member and manufacturing method of sliding member |
abstract |
PROBLEM TO BE SOLVED: To prevent peeling of a solid lubricant. In a sliding member having a sliding surface coated with a plating film, a cavity is formed in the plating film, and a crack communicating with the cavity is formed on the surface of the plating film. The hollow portion communicating with the crack is filled with a solid lubricant. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014074585-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015199189-A1 |
priorityDate |
2005-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |