abstract |
PROBLEM TO BE SOLVED: To provide a lubricating coating composition that uses a thermosetting resin that is not subject to regulations due to environmental problems and can be formed into a film by heating at a relatively low temperature, has low friction and low wear, and has excellent corrosion resistance. SOLUTION: One or both of furfural and furfuryl alcohol is used as a starting material, and a furan resin initial condensate that becomes a low-friction furan resin by curing, and three types of molybdenum disulfide, polytetrafluoroethylene, and graphite. A lubricating coating composition comprising a solid lubricant dispersed in an organic solvent. The blending amount of the furan resin initial condensate is preferably 30 to 65% by weight of the entire composition. [Selection figure] None |