Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-405 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 |
filingDate |
2005-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b0a7295d391808286590e0bc442bee1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_102e74facdf8a8c17fb33c783780f910 |
publicationDate |
2007-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007002183-A |
titleOfInvention |
Silicone rubber composition for tire production and method for producing the same |
abstract |
PROBLEM TO BE SOLVED: To produce a tire having improved shape stability, strength, elongation and creep resistance as compared with conventional polysulfide rubber liquid rubber, and further improved notch property (crack resistance) inherent to silicone rubber. A silicone rubber composition is provided. (A) 100 parts by weight of a linear diorganopolysiloxane containing a specific alkenyl group, (B) 1-20 parts by weight of an organohydrogenpolysiloxane containing a specific hydrogen atom, (C) ratio 30 to 60 parts by weight of silica fine powder having a surface area of 50 m 2 / g or more, (D) 0.5 to 20 weights of linear diorganopolysiloxane containing a specific alkenyl group and having a weight average molecular weight smaller than that of component (A) Part and (E) platinum group metal-based catalyst (A), (B) and (D) composition containing 5 to 300 ppm in terms of weight of platinum group metal with respect to the total amount of components, (D) component And the component (E) are previously mixed uniformly, and then the mixture is mixed with the remaining components. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101701848-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009073980-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009256507-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009132809-A |
priorityDate |
2005-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |