http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006522218-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-3605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-40 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-36 |
filingDate | 2004-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006522218-A |
titleOfInvention | Method for forming a surface-modified workpiece |
abstract | PROBLEM TO BE SOLVED: To achieve an equal or improved corrosion resistance and adhesion mediation by means of an aluminum or aluminum alloy, which is adhesion-improved and / or corrosion-protected in an inexpensive manner, in particular reduced grain formation. A method is provided that results in a workpiece that is superior in structure compared to previously formed aluminum or aluminum alloy workpieces. A metal and / or one comprising preparing a workpiece to be modified and treating the workpiece with at least one modifying means to obtain a surface-modified workpiece. Alternatively, a method of forming a surface-modified workpiece comprising a plurality of alloys, wherein the prepared workpiece to be surface-modified has a temperature of 40 to 700 ° C., in particular 80 to 550 ° C., and at least One means for modifying has a temperature of at least −200 ° C., in particular at least 0 ° C. and a maximum of 100 ° C., in particular a maximum of 80 ° C. An apparatus for bonding at least two workpieces by material bonding in order to carry out the method described above. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019173592-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7045236-B2 |
priorityDate | 2003-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 69.