http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006342281-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95136e4276343dbae035a63330dabfc7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14 |
filingDate | 2005-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f82d41fbd75fe7065180406ee8a0541c |
publicationDate | 2006-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006342281-A |
titleOfInvention | Polyester resin for binder fiber |
abstract | PROBLEM TO BE SOLVED: To provide a polyester resin which is excellent in biodegradability and can be processed into a soft fiber structure. [Solution] Polyester comprising ethylene glycol as a main diol component, with respect to the total acid component, terephthalic acid is 50 to 80 mol%, isophthalic acid is 10 to 40 mol%, aliphatic dicarboxylic acid is 3 to 30 mol%, The phosphorus compound represented by the formula (1) is copolymerized in an amount of 0.3 to 1.5 mol%, has a glass transition temperature of 40 to 80 ° C. or higher, and a softening temperature of 80 to 180 ° C. Polyester resin for binder fibers. [Chemical 1] [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101512288-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102003888-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013189550-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190013234-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011093986-A |
priorityDate | 2005-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 98.