http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006307400-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e17106754fea38d7e6d5d768764d628b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27N3-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D197-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21J1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21B1-14 |
filingDate | 2005-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54c87338c77de639134f5a0433b3d6b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06f7cc25cfbfa2d36bac3611ea61865e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3781ab6b9d5c464175712c0c34a100c |
publicationDate | 2006-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006307400-A |
titleOfInvention | Liquid lignocellulose and production method and use thereof |
abstract | PROBLEM TO BE SOLVED: To obtain a long fiber bundle because ground pulp, which is a typical liquid lignocellulose, is manufactured by grinding logs and chips with a grinder or a referrer. Lignin and fine lignocellulose are discarded. In liquified wood and lignocellulose, lignocellulose is liquefied by consuming high temperature and high pressure energy and chemicals, not lignocellulose itself. SOLUTION: Lignocellulose chips are mixed with water and solvent, and wet pulverization is performed with closed or circulatory machines and systems to discharge waste without using high-temperature and high-pressure energy and chemicals. Without being carried out, lignocellulose having a fine particle size, preferably liquid lignocellulose in which lignocellulose having an average particle size of 30 μm or less is dispersed can be obtained, and when dried, a strong film is formed, and a paint, molded product, fiber It can be used as a treatment agent. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114474754-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114368053-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010053282-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012111063-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016532015-A |
priorityDate | 2005-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 36.