Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_98572b2dbf95b554ecb4a24bc9d3958a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 |
filingDate |
2005-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9728e7e3922ceb2c5a002a9b6325a76 |
publicationDate |
2006-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006297322-A |
titleOfInvention |
Coating film forming method, paint, release material and rubber material |
abstract |
PROBLEM TO BE SOLVED: To improve the durability of a coating film containing a resin, and to form a coating film on the surface of the rubber material 10 by applying a coating material 20 containing a solvent for swelling the rubber and the resin to the surface of the rubber material. , Is adopted. [Selection] Figure 1 |