Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a6638ac6b1020cd2c62d09d748bc1ab9 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02 |
filingDate |
2005-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_987079fe9744d0944086be51eabea2bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75d5ea53c147f7e998ef6a559e0892d1 |
publicationDate |
2006-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006297230-A |
titleOfInvention |
Titanium oxide thin film, photocatalytic material including titanium oxide thin film, method for producing the same, photocatalytic water purification device, and water purification method utilizing photocatalytic reaction |
abstract |
PROBLEM TO BE SOLVED: To provide a photocatalytic material comprising a titanium oxide thin film having a roughness suitable as a photocatalyst, which is a highly reliable titanium oxide thin film that does not cause peeling or cracking on a conductive substrate such as metal, and its An object is to provide a manufacturing method. Another object of the present invention is to provide a water purification device containing the photocatalytic material and a method for purifying the water. Titanium oxide is formed on a cathode electrode by performing electrophoretic electrodeposition on a conductive substrate such as metal using a titanium oxide-IPA suspension subjected to ultraviolet irradiation under predetermined conditions. By simultaneously forming a film and generating gas derived from IPA, a titanium oxide thin film having a roughness suitable as a photocatalyst on the surface of the coating film is produced. [Selection] Figure 3 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011098312-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-200490656-Y1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015079594-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008302328-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009256790-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011120967-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111758541-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111758541-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190002657-U http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015104690-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10406516-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008221088-A |
priorityDate |
2005-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |