Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60R21-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60R21-20 |
filingDate |
2005-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_076a4236f8cc83189dda29901d6ca122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f89d6723c697b7d58a60a60a1ac7c5d |
publicationDate |
2006-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006282992-A |
titleOfInvention |
Method for producing thermoplastic elastomer composition and airbag cover |
abstract |
An airbag cover excellent in low-temperature impact strength and a method for producing a thermoplastic elastomer composition suitable for producing the airbag cover are provided. At least the following component (A) 10 to 50% by weight, component (B) 20 to 60% by weight, and component (C) 20 to 60% by weight are dynamically mixed in the presence of a crosslinking agent. A method for producing a thermoplastic elastomer composition comprising a step of cross-linking to (the total of component (A), component (B) and component (C) is 100% by weight): (A) Oil-extended ethylene-α-olefin-nonconjugated diene copolymer rubber having a density of 850 to 900 kg / m 3 and a Mooney viscosity (ML 1 + 4 100 ° C.) of 30 to 150; (B) an ethylene-α-olefin copolymer having a density of 850-910 kg / m 3 and a melt flow rate measured at 230 ° C. under a load of 21.18 N of 0.1-80 g / 10 min; (C) Polypropylene resin [selection drawing] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113383037-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020162382-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7293261-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160016580-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9388305-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020162382-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7361773-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10253172-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8686088-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010537039-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012224837-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102201012-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013173818-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016035043-A |
priorityDate |
2005-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |