http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006274225-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5e5c121269689cbab9b3a4548b15caf3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-22 |
filingDate | 2005-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_120b766608e23952be77ca3521b40cb9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_28ac49e90d167e75e7252903f74016f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c96bede285096c1e44772f17da0b48ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24f7a2df22e6d3ce04ca23e4cc1a0833 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c1047ad06c18088623861e29eb2cde4 |
publicationDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006274225-A |
titleOfInvention | Thermally decomposable fluorine-containing (meth) acrylic acid ester polymer and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To melt PTFE, a high temperature is required, and since the viscosity at the time of melting is very high, it is difficult to apply a general molding process, and its use is limited. A resin capable of solving such problems has been desired. As a result of intensive studies in view of the above problems, the present inventors have found that a 10% weight reduction temperature of a specific structure is 350 ° C. or more, and a fluorine atom-containing (meth) acrylic acid ester A polymer or a method for producing the same is provided. [Selection figure] None |
priorityDate | 2005-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |