http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006274193-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-232 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 2005-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_588927b09998fe1646bc49317b75a63f |
publicationDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006274193-A |
titleOfInvention | Pre-expanded thermoplastic resin particles and in-mold foam |
abstract | [PROBLEMS] To increase mechanical strength when pre-expanded particles and then a foamed molded article are produced from a thermoplastic resin composition in which a layered inorganic compound organized into a polyolefin resin and a functional group-containing polyolefin resin is blended. To do. SOLUTION: It comprises (A) a polyolefin resin, (B) a functional group-containing polyolefin resin satisfying specific conditions, and (C) an organically layered inorganic compound, and (A) component and (B) component 100 weight. The density is 10 kg / m 3 or more and 300 kg using thermoplastic resin pre-expanded particles obtained by foaming particles made of a thermoplastic resin composition containing 1 to 20 parts by weight of component (C) as inorganic weight with respect to parts. / M 3 or less in-mold foam molded article is produced. [Selection figure] None |