http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006274075-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b576861ef2bbff1956483170b6360884 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10B29-06 |
filingDate | 2005-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fccdd9ab2bb214bdb97a75f94e1c27b2 |
publicationDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006274075-A |
titleOfInvention | Coke oven wall repair method |
abstract | 【wrap up】 [Problem] By stabilizing the powder concentration of the dry seal material in the carbonization chamber in a short time, repair by the dry seal method can be carried out stably in a short time regardless of the crack location in the furnace wall, and fire resistance Provided is a method for repairing a coke oven wall that can reduce the consumption of wood powder. SOLUTION: A refractory powder from a refractory powder tank installed in a coal-fired car of a coke oven, together with a pressurized gas, is extruded at the upper part of a carbonization chamber from an extruder side to a fire-fighting car side in a row of coal charge inlets. Blowing into the carbonization chamber from the first or second coal inlet from one side, exhausting from the first or second coal inlet from the other side, and installing the refractory powder contained in the exhaust It is collected by the dust collector installed in the charcoal car and returned to the refractory powder tank. [Selection] Figure 1 |