http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006250979-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4af0df9a26ff4aafde7285cbd8eb12f4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G7-00 |
filingDate | 2005-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb65781be234f2f9cd29bef0141b7110 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_984c2f2ee65a6e35363b573b2cfb27c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33ebc676d0a70e78432c99b16631c789 |
publicationDate | 2006-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006250979-A |
titleOfInvention | Image forming apparatus |
abstract | PROBLEM TO BE SOLVED: To obtain a high-gloss toner image similar to a granular silver salt photographic print while preventing the occurrence of a bruster or an offset phenomenon of a base material on the premise of a two-stage fixing method, and further, after image formation Maintains high gloss even during heat storage. A composition and a melting point condition of a toner 3 are determined, and a fixing device 4 includes a first fixing device 5 that primarily fixes a toner image G on a substrate 1 without melting a toner receiving layer 1b, and a base. And a second fixing device 6 for melting and fixing the toner 3 and the toner receiving layer 1b so as to give gloss to the toner image G primarily fixed on the material 1, and the fixing temperature of the first fixing device 5 Is T1 (° C.) and the fixing temperature of the second fixing device 6 is T2 (° C.), Tm <T1 <Tm + 20, the toner viscosity at T1 is less than 10 4.5 Pa · s, and the toner receiving layer at T1 The toner satisfies the fixing conditions of a viscosity of 10 6 Pa · s or more and a viscosity of the toner receiving layer at T 2 of 10 to 10 3.5 Pa · s. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010145508-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008310248-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011528811-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014160194-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014224862-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9429890-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016224249-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008116846-A |
priorityDate | 2005-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 109.