http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006249363-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 |
filingDate | 2005-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d7b245db2469622b460637744ecfc96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08a9a321df548c072a0016ef647762c0 |
publicationDate | 2006-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006249363-A |
titleOfInvention | Rubber composition and pneumatic tire using the same |
abstract | Provided is a rubber composition that can be used for a tread rubber of a tire to improve the steering stability, fracture characteristics, and wear resistance of the tire. SOLUTION: A styrene-butadiene copolymer rubber (A) having a polystyrene equivalent weight average molecular weight of 300,000 to 4,000,000, 60 to 95% by mass, a polystyrene equivalent weight average molecular weight of 400,000 or more, and a cis-1,4 bond content of 90%. The liquid styrene-butadiene copolymer (C) having a polystyrene-equivalent weight average molecular weight of 5,000 to 200,000 is 10 to 100 parts by mass of the rubber component consisting of 5 to 40% by mass of the above polyisoprene rubber (B). A rubber composition is formed by blending 200 parts by mass. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008120895-A |
priorityDate | 2005-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 128.