abstract |
Provided is a highly fluid non-shrink mortar that has higher fluidity than conventional non-shrink mortars, can be filled even in gaps with a spacing of less than 20 mm, is less likely to cause material separation, and has high cured product compressive strength. . A JA funnel flow time of fresh mortar is 20 to 40 seconds, a flow value according to JASS 15M-103 “Quality Standard of Self-Leveling Material” is 16 to 22 cm, and a 28-day compression strength of a cured product is 50 to 70 N. / Mm 2 high fluidity non-shrinking mortar, so it has higher fluidity than conventional non-shrinking mortar, and it is difficult to cause material separation even though the gap can be filled in a gap of less than 20 mm. . Moreover, the cured product has a high compressive strength. [Selection] Figure 1 |