abstract |
To provide a method for producing an acrylic resin composition film excellent in transparency, defect-free property, and optical isotropy. An acrylic resin composition solution containing an acrylic resin composition and an organic solvent is applied onto a support, and after drying, the support and the acrylic resin composition coating film are peeled to obtain an acrylic resin composition film. In the method, when the residual solvent amount in the acrylic resin composition coating film is 5% by mass or less, the support is fixed and the support and the acrylic resin composition coating film are peeled off, 180 ° of the coating film with respect to the support The peeling force is 0.5 to 5 g / 25 mm. [Selection figure] None |