Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N17-00 |
filingDate |
2005-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f997e70f60b97dcfd9d8f49169064471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ade1f6124e1170eee39cea04f7f5c566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46712ff5693b7b62c3af6b2e0533c35c |
publicationDate |
2006-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006234421-A |
titleOfInvention |
Accelerated testing method for stress corrosion cracking |
abstract |
PROBLEM TO BE SOLVED: To provide an accelerated test method for stress corrosion cracking capable of evaluating characteristics of stress corrosion cracking generated in the atmosphere or in an aqueous solution due to chloride in a short period of time. A test piece loaded with stress is placed in an aqueous solution containing a drug having an action of suppressing pitting corrosion and chloride ion Cl - and having a pH of 4 to 9, and the test piece is energized. The stress corrosion cracking test is accelerated by measuring the time until the specimen breaks due to electrolytic action. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113005457-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011038094-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111398001-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4690279-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008076297-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010127749-A |
priorityDate |
2005-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |